DGK Pellachrom | decorative and marine paints | - Header Section

DGK Pellachrom | decorative and marine paints | - Main Section

DGK Pellachrom | decorative and marine paints | - Main Component

water
SOLVENT BASED
  • 750 ml
  • 2.5 L

POLYGLOSS

Header

polyurethane top coat

Premium two-part polyurethane top coat, extremely resistant to adverse weather conditions. Long-lasting bright colours with excellent yellowing resistance. Excelling durable gloss. Gives an extremely tough and elastic surface with great resistance to tear and knocks while it creates a flawless finish. Its composition ensures excellent results on all surfaces. Ideal for indoor and outdoor use on highly demanding surfaces. Ideal for any type of boat.

  • premium high-gloss finish
  • long-lasting shades
  • extreme chemical and mechanical resistance
xrisi4xrisi4
BUILDINGS
INTERIOR-EXTERIOR USE
xrisi4xrisi4
FREEBOARDS - UNDERWATER HULL
highgloss
Finish
toolsall
TOOLS
POLYGLOSS
THINNING
1 hr
DRYING TIME
2-4 hrs
OVERCOATING INTERVAL
2
RECOMMENDED COATS
14 sin plin 2
m2/L
SPREADING RATES
water READY TO USE COLOR SHADES pdf icon

Preparation

Carefully prepare surface to obtain good results. Remove all weathered coatings, rust and oils. Sand and remove sanding residue with a rag.

New polyester:
Degreasing new polyester is of utmost importance. Please follow the proposed procedure: Wash surface with warm water and soap (detergent). Rinse well, allow to dry and clean using a thinner. Sand and remove sanding residue with a whisk and a thinner soaked rag. The surface is now ready to be painted. Any other surface preparation method could trap grease inside the surface thus, rendering painting impossible. Prime with UNI-PRIMER, 1-2 coats. Apply 2 coats of POLYGLOSS.
New plaster, concrete, brick, cement and stone:
Apply POLACRYL 301 until surface saturation is achieved. Prime with UNI-PRIMER, 1-2 coats. Apply 2-3 coats of POLYGLOSS.
New wood:
Apply POLACRYL 301 until surface saturation is achieved. Prime with UNI-PRIMER, 1-2 coats. Apply 2-3 coats of POLYGLOSS.
New metal:
Prime with X-RUST, 2 coats. Apply 2-3 coats of POLYGLOSS.
New glass, tiles, enamel plates:
Prime with SMALTO GRIP, 1-2 coats. Apply 2-3 coats of POLYGLOSS.
Recoated old surfaces:
Prime with UNI-PRIMER, 1-2 coats. Apply 2-3 coats of POLYGLOSS.

Use

► Stir well component A before use to achieve homogeneity. Then, add component B progressively while constantly stirring.
► Make sure your tool has the adequate quantity of paint to cover an entire section. This practice should be strictly followed to obtain optimum results.
► Sand surface smooth with the right sandpaper for the task before painting.
► To prevent bubble forming during application, work in an area protected against direct sunlight if possible.
► Do not apply when ambient temperature and surface temperature is below 10°C, above 35°C and when relative humidity is above 70%.
► To improve the chemical resistance and the mechanical properties of the final surface, add ADDITIVE 640 before application of the last coat.
► Make sure that the colour of the support is perfectly covered before application of POLYGLOSS mixed with ADDITIVE 640.
► Adequate ventilation must be ensured due to the hazardous fumes generated during paint application.

Drying out - coverage

Drying times are dependent on ambient temperature and film thickness.

Touch dry: 1 hour.

Recoat: 2-4 hours.

Practical coverage: 12-16m²/lt depending on the thickness of each coat and the surface porosity. 

DGK Pellachrom | decorative and marine paints | - Bottom info

Calculate the quantity of the paint

you need for